<math>N\,\!</math>  is chromophore number density
<math>N\,\!</math>  is chromophore number density


<math><cos^3\theta>\,\!</math>  is  the acentricity
<math><cos^3\theta>\,\!</math>  is  the acentricity or order parameter




=== Figure of Merit ===
=== Figure-of-Merit ===


Figure of merit: r33 preferably > 1000 pm/V
Figure-of-merit: r33 preferably > 1000 pm/V


Current Status: 600pm/V
Current Status: 600pm/V
Line 20: Line 20:
For poled polymers for THz generation and detection  
For poled polymers for THz generation and detection  


Figure of merit: r33 preferably > 350 pm/V
Figure-of-merit: r33 preferably > 350 pm/V


Current Status: 600pm/V
Current Status: 600pm/V
=== Measurement ===
[[Teng-Mann Method]]
[[Attenuated Total Reflectance]]

Latest revision as of 10:21, 8 November 2011

r33 (pronounced "r three three") also called the electro-optic coefficient is a measure of the changability optical activity of a material when an electric field is applied.

<math>r_{33} = \beta(\epsilon,\omega)N<cos^3\theta>\,\!</math>

where

<math>\beta(\epsilon,\omega)\,\!</math> is the molecular first hyperpolarizability which at a give wavelenth ω

<math>N\,\!</math> is chromophore number density

<math><cos^3\theta>\,\!</math> is the acentricity or order parameter


Figure-of-Merit

Figure-of-merit: r33 preferably > 1000 pm/V

Current Status: 600pm/V

For poled polymers for THz generation and detection

Figure-of-merit: r33 preferably > 350 pm/V

Current Status: 600pm/V